Tube profile machining process

US9463527B2 · kind B2 · utility

1Cited by
16References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 29, 2013
Grant dateOct 11, 2016
Priority date
Expiry dateApr 18, 2034

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB23K2103/10
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

In a first embodiment, at a time of magnetic pulse welding, a stepped tube profile machining process axially bores a walled tube from an end inward to a transition depth to form a section with a reduced wall thickness and then axially bores the walled tube from the transition depth to a fall off depth, thereby forming a section with a maximized welding wall section. In a second embodiment, also at a time of magnetic pulse welding, a surface angle tube profile machining process axially bores at a surface angle a walled tube from an end to a bore length to form an angular welding wall thickness inward to a maximized wall section. For both embodiments, the bored surfaces are virgin with no pits, oil, residue, or oxidation thereon, thus making the machined walled tubes available for immediate magnetic pulse welding.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.