Continuous casting method for ingot produced from titanium or titanium alloy
US9475114B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 10, 2014 |
| Grant date | Oct 25, 2016 |
| Priority date | — |
| Expiry date | Jan 10, 2034 |
Classification
- Technology area (CPC F)Mechanical Engineering; Lighting; Heating
- CPC primaryF27D2099/0031
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
By controlling the temperature (TS) of a surface portion (11a) of an ingot (11) in a contact region (16) between a mold (2) and the ingot (11) and/or a passing heat flux (q) from the surface portion (11a) of the ingot (11) to the mold (2) in the contact region (16), the thickness (D) in the contact region (16) of a solidified shell (13) obtained by the solidification of molten metal (12) is brought into a predetermined range. Consequently, an ingot having a good casting surface state can be cast.