Sulfur-modified chloroprene rubber composition and molded body
US9475895B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Sep 10, 2013 |
| Grant date | Oct 25, 2016 |
| Priority date | — |
| Expiry date | Sep 10, 2033 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08K3/06
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
An object of the invention is to provide a sulfur-modified chloroprene rubber composition improved in heat resistance. A sulfur-modified chloroprene rubber composition, comprising a sulfur-modified chloroprene rubber containing sulfur chemically bound thereto and sulfur not chemically bound to the sulfur-modified chloroprene rubber, wherein: the ratio of the amount of sulfur chemically bound to the sulfur-modified chloroprene rubber to the total amount of sulfur in the sulfur-modified chloroprene rubber composition (amount of chemically bound sulfur [mass %]/total amount of sulfur [mass %]) is 0.1 to 0.45; and the sulfur-modified chloroprene rubber has, at the molecular terminal, at least one structure represented by the following General Formula (1) or (2): —S—C(═S)—O—R1 . . . (1) (in General Formula (1), R1 represents an alkyl group having 1 to 4 carbon atoms) or —S—R2 . . . (2) (in General Formula (2), R2 represents an alkyl group having 8 to 20 carbon atoms).
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.