Patent · US Active

Sulfide solid electrolyte material, lithium solid-state battery, and method for producing sulfide solid electrolyte material

US9484597B2 · kind B2 · utility

5Cited by
3References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 21, 2015
Grant dateNov 1, 2016
Priority date
Expiry dateAug 21, 2035

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02T10/70
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A sulfide solid electrolyte material contains glass ceramics that contains Li, A, X, and S, and has peaks at 2θ=20.2° and 23.6° in X-ray diffraction measurement with CuKα line. A is at least one kind of P, Si, Ge, Al, and B, and X is a halogen. A method for producing a sulfide solid electrolyte material includes amorphizing a raw material composition containing Li2S, a sulfide of A, and LiX to synthesize sulfide glass, and heating the sulfide glass at a heat treatment temperature equal to or more than a crystallization temperature thereof to synthesize glass ceramics having peaks at 2θ=20.2° and 23.6° in X-ray diffraction measurement with CuKα line, in which a ratio of the LiX contained in the raw material composition and the heat treatment temperature are controlled to obtain the glass ceramics.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.