Patent · US Active

Flux-cored arc welding wire for providing superior toughness and weldability to a welded joint at a low temperature, and welded joint using same

US9492894B2 · kind B2 · utility

0Cited by
1References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 27, 2011
Grant dateNov 15, 2016
Priority date
Expiry dateJan 9, 2033

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/005
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

Provided are a flux cored arc welding wire able to improve low-temperature toughness of a weld joint and a weld joint using the same, in which the flux cored arc welding wire includes 0.01 wt % to 0.1 wt % of carbon (C), 0.3 wt % to 1.4 wt % of silicon (Si), 1.0 wt % to 3.0 wt % of manganese (Mn), 4.0 wt % to 7.5 wt % of titanium (Ti)+TiO, 0.01 wt % to 3.0 wt % of nickel (Ni), 0.01 wt % to 0.2 wt % of boron (B), 0.02 wt % to 0.42 wt % of yttrium (Y) or 0.02 wt % to 0.56 wt % of a rare earth metal (REM), and iron (Fe) as well as other unavoidable impurities as a remainder.