Frictional weld joint for an article comprising a thermoplastic material

US9539758B2 · kind B2 · utility

0Cited by
25References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 23, 2013
Grant dateJan 10, 2017
Priority date
Expiry dateMay 23, 2033

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T403/477
  • WIPO fieldOther special machines
  • WIPO sectorMechanical engineering

Abstract

A frictional weld joint couples together first and second body portions of an article. The first body portion has a first nominal wall thickness and a first joint surface. The second body portion has a second nominal wall thickness and a second joint surface. A total bead height is defined between the joint surfaces. A first bead extends from the first joint surface defining a first bead height. A second bead extends from the second joint surface and is coupled to the first bead. A final second bead height is defined between the first bead and the second joint surface. A ratio of the first bead height to the final second bead height is of from about 0.40 to about 1.70. A ratio of the total bead height to at least one of the first and second nominal wall thicknesses is equal to or less than 6.00.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.