Patent · US Active

Preparation process of transition metal boride and uses thereof

US9546095B2 · kind B2 · utility

0Cited by
2References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 22, 2014
Grant dateJan 17, 2017
Priority date
Expiry dateJan 22, 2034

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC25C3/12
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The invention provides a preparation process of transition metal boride, comprising the following steps: A) aluminum is put in a reactor, inert gas is fed into the reactor after evacuation, the reactor is heated up to 700 to 800° C. and then added with dry potassium fluoborate or sodium fluoborate, monomer boron and cryolite are generated by rapid stirring and reaction for 4 to 6 hours, and the molten liquid at the upper layer is sucked out and the monomer boron is obtained by means of separation; and B) the obtained monomer boron is added with transition metal for reaction at the temperature from 1800 to 2200° C. in order to generate corresponding transition metal boride.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.