High-strength electric-resistance-welded steel pipe of excellent long-term softening resistance in intermediate temperature ranges

US9551047B2 · kind B2 · utility

0Cited by
0References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 17, 2013
Grant dateJan 24, 2017
Priority date
Expiry dateAug 5, 2033

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/13
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A high strength electric resistance welded steel pipe has a yield strength of 450 MPa or more and excellent resistance to softening for a long period in an intermediate temperature range and a method of manufacturing the steel pipe are provided. The steel pipe has a chemical composition containing, by mass%, C: 0.026% or more and 0.084% or less, Si: 0.10% or more and 0.30% or less, Mn: 0.70% or more and 1.90% or less, Al: 0.01% or more and 0.10% or less, Nb: 0.001% or more and 0.070% or less, V: 0.001% or more and 0.065% or less, Ti: 0.001% or more and 0.033% or less, Ca: 0.0001% or more and 0.0035% or less, in which the condition that Pcm is 0.20 or less is satisfied.