Porous composite metal oxide, catalyst using the same, and methods for producing the porous composite metal oxide and the catalyst

US9556023B2 · kind B2 · utility

4Cited by
4References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 10, 2010
Grant dateJan 31, 2017
Priority date
Expiry dateNov 14, 2032

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/16
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A porous composite metal oxide, including a mixture of first ultrafine particles containing alumina and second ultrafine particles containing zirconia, wherein the first ultrafine particles and the second ultrafine particles are uniformly dispersed in such a way as to satisfy a condition that standard deviations of content ratios (% by mass) of all metal elements contained in the porous composite metal oxide at 0.1% by mass or more are each 10 or less, the standard deviations being obtained by measuring content ratios of the metal elements at 100 measurement points within a minute analysis region of 20 nm square by energy dispersive X-ray spectroscopy using a scanning transmission electron microscope equipped with a spherical aberration correction function.