Abstract

A low dielectric constant glass fiber, in mass percentage, includes 50%˜60% of SiO2, 10%˜20% of Al2O3, 12%˜20% of B2O3, 0˜4% of CaO, 4%˜10% of MgO, 0.1%˜0.5% of Na2O+K2O, 0˜0.5% of Li2O, 0.2%˜3% of F2 and 0˜0.2% of Fe2O3. Compared with the related art, the glass composition contains higher content of SiO2, which can greatly reduce dielectric properties of the glass fiber. Meanwhile, a small amount of F2 is added thereto, which not only can effectively improve the fiberizing temperature of the glass fiber but also can reduce glass viscosity and density and reduce glass refractive index and dielectric properties. In addition, lower content of CaO is further contained, but almost no alkali metal particles such as Na2O+K2O are contained, which further reduces the dielectric properties of the glass fiber.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.