Patent · US Active

Method of making high performance activated aluminum sesquichlorohydrate powders

US9572758B2 · kind B2 · utility

2Cited by
9References
17Claims
0Family size

Assignee

Inventor

Key dates

Filing dateJun 30, 2015
Grant dateFeb 21, 2017
Priority date
Expiry dateJun 30, 2035

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/90
  • WIPO fieldPharmaceuticals
  • WIPO sectorChemistry

Abstract

Activated aluminum sesquichlorohydrate (AASCH) powders and method of making are disclosed. The AASCH powder has Al:Cl atomic ratio of from about 1.60 to about 1.90 and Band III polymer concentration of at least about 20% and Band IV polymer concentration of at least about 15% when analyzed with Size Exclusion Chromatogram (SEC) operated by High Performance Liquid Chromatograph (HPLC). The method of making the active comprises (a) diluting the concentrated aluminum sesquichlorohydrate (ASCH) solution to from about 10% to about 25% by weight and (b) heating the diluted solution to obtain a Band III polymer concentration of at least about 20% and a Band IV polymer concentration of at least about 15%, and (c) drying the heated solution to powders having Al:Cl ratio of about 1.60 to about 1.90 and (d) optionally screen or light mill the powders to free flowing spherical particles.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.