Patent · US Active

Copolymers

US9587055B2 · kind B2 · utility

7Cited by
3References
24Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 4, 2009
Grant dateMar 7, 2017
Priority date
Expiry dateJul 7, 2030

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/139
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Copolymers comprising ethylene and alpha-olefins having (a) a density (D) in the range 930-960/g/m3 (b) a melt index (MI2) in the range 0.1-3.5 g/10 min (c) a melt elastic modulus G′ (G″=500 Pa) in the range 40 to 150 Pa, and (d) a ratio of complex dynamic shear viscosities η*(0.1)/η(100) in the range 1.5 to 5.5. The copolymers are suitable for use as Polyethylenes of Raised Temperature Resistance (PE-RT) for use in hot water piping systems. The copolymers may be prepared by use of meltallocene catalyst systems. Pipes having a time to failure of ≧500 hrs measured according to ISO 1167 at 110° C. and 2.6 MPa prepared in a single reactor are also disclosed.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.