Blow molded article with good mechanical and optical properties
US9587097B2 · kind B2 · utility
0Cited by
0References
17Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Dec 18, 2014 |
| Grant date | Mar 7, 2017 |
| Priority date | — |
| Expiry date | Dec 18, 2034 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L2205/025
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
Blow molded article comprising a propylene copolymer having a MFR2 (230° C.) in the range of more than 2.0 to 12.0 g/10 min, a comonomer content in the range of 4.0 to below 4.0 mol.-%, a melting temperature in the range of 125 to below 143° C., and a xylene cold soluble fraction (XCS) in the range of above 15.0 to 40.0 wt.-%.