Composite cathode active material, method of preparing the composite cathode active material, and cathode and lithium battery each including the composite cathode active material
US9601761B2 · kind B2 · utility
0Cited by
0References
15Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Apr 25, 2014 |
| Grant date | Mar 21, 2017 |
| Priority date | — |
| Expiry date | Sep 27, 2034 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A composite cathode active material, a method of preparing the composite cathode active material, a cathode including the composite cathode active material, and a lithium battery including the cathode. The composite cathode active material includes a lithium intercalatable material; and a garnet oxide, wherein an amount of the garnet oxide is about 1.9 wt % or less, based on a total weight of the composite cathode active material.