Crystallized glass and method for manufacturing same

US9611170B2 · kind B2 · utility

0Cited by
7References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 9, 2014
Grant dateApr 4, 2017
Priority date
Expiry dateJan 9, 2034

Classification

  • Technology area (CPC G)Physics
  • CPC primaryG02B6/12007
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

What is achieved is an optical wavelength multiplexer/demultiplexer not necessarily requiring the function of adjusting the optical path. A value (ΔLmax−ΔLmin)/L obtained by dividing a difference between a maximum value ΔLmax and a minimum value ΔLmin of ΔL in a range of −40° C. to 80° C. by L is 8×10−6 or less where L represents a length of a crystallized glass (1) at 30° C. and ΔL represents a difference between a length (Lt) of the crystallized glass (1) at each of the temperatures and the length (L) thereof at 30° C.