Abstract
Described is a clearcoat coating composition, its use, and a process for preparing the clearcoat coating composition. The clearcoat coating composition comprises (A) at least one polyester having an OH number of 80-250 mg KOH/g; (B) at least one butanol-etherified melamine-formaldehyde resin having a crosslinking onset temperature between 65° C.-100° C. lower than the crosslinking onset temperature of hexamethoxy-methylmelamine; (C) at least one butanol-etherified melamine-formaldehyde resin having a crosslinking onset temperature between 30° C.-60° C. lower than the crosslinking onset temperature of hexamethoxymethylmelamine; (D) at least one organic urea compound as rheological assistant; and (E) at least one acid catalyst.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.