Patent · US Active

Low friction coatings with improved abrasion and wear properties and methods of making

US9617654B2 · kind B2 · utility

19Cited by
7References
39Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 21, 2012
Grant dateApr 11, 2017
Priority date
Expiry dateOct 26, 2033

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/24975
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

Provided are low friction coatings with improved abrasion, wear resistance and methods of making such coatings. In one form, the coating includes: i) an under layer selected from the group consisting of CrN, TiN, TiAlN, TiAlVN, TiAlVCN, TiSiN, TiSiCN, TiAlSiN and combinations thereof, wherein the under layer ranges in thickness from 0.1 to 100 μm, ii) an adhesion promoting layer selected from the group consisting of Cr, Ti, Si, W, CrC, TiC, SiC, WC, and combinations thereof, wherein the adhesion promoting layer ranges in thickness from 0.1 to 50 μm and is contiguous with a surface of the under layer, and iii) a functional layer selected from the group consisting of a fullerene based composite, a diamond based material, diamond-like-carbon and combinations thereof, wherein the functional layer ranges from 0.1 to 50 μm and is contiguous with a surface of the adhesion promoting layer.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.