Amorphous cathode material for battery device
US9627709B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 15, 2014 |
| Grant date | Apr 18, 2017 |
| Priority date | — |
| Expiry date | Jan 11, 2035 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P70/50
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A method of fabricating a multilayered thin film solid state battery device. The method steps include, but are not limited to, the forming of the following layers: substrate member, a barrier material, a first electrode material, a thickness of cathode material, an electrolyte, an anode material, and a second electrode material. The formation of the barrier material can include forming a polymer material being configured to substantially block a migration of an active metal species to the substrate member, and being characterized by a barrier degrading temperature. The formation of cathode material can include forming a cathode material having an amorphous characteristic, while maintaining a temperature of about −40 Degrees Celsius to no greater than 500 Degrees Celsius such that a spatial volume is characterized by an external border region of the cathode material. The method can then involve transferring the resulting thin film solid state battery device.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.