Polyurethane article with increased comfort

US9670307B2 · kind B2 · utility

1Cited by
26References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 12, 2010
Grant dateJun 6, 2017
Priority date
Expiry dateApr 12, 2030

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08G2350/00
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A unique combination of a hydrophilic polyol (A) and a hydrophobic polyol (B) having a terminal ethylene oxide cap are used in a resin composition and a polyurethane system, and are used to form a polyurethane article, such as a polyurethane foam. The hydrophilic polyol (A) is ethylene oxide (EO) rich and the hydrophobic polyol (B) is propylene oxide (PO) rich. The hydrophilic polyol (A) and the hydrophobic polyol (B) are present in the resin composition and the polyurethane system in a weight ratio (A:B) of from 1.5:1 to 20:1. The polyurethane article exhibits excellent comfort for use in vehicle applications, such as automotive and motorcycle seating, due to reduced resonance frequency and reduced peak vibration transmissivity relative to previous polyurethane articles.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.