Resorbable macroporous bioactive glass scaffold and method of manufacture
US9707079B2 · kind B2 · utility
2Cited by
10References
16Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | May 27, 2016 |
| Grant date | Jul 18, 2017 |
| Priority date | — |
| Expiry date | May 27, 2036 |
Classification
- Technology area (CPC A)Human Necessities
- CPC primaryA61F2310/00329
- WIPO fieldMedical technology
- WIPO sectorInstruments
Abstract
A method of manufacturing a resorbable, macroporous bioactive glass scaffold comprising approximately 24-45% CaO, 34-50% SiO2, 0-25% Na2O, 5-17% P2O5, 0-5% MgO and 0-1% CaF2 by mass percent, produced by mixing with pore forming agents and specified heat treatments.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.