Patent · US Active

Wicking nonwoven mat from wet-laid process

US9716293B2 · kind B2 · utility

0Cited by
2References
23Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 9, 2015
Grant dateJul 25, 2017
Priority date
Expiry dateMar 23, 2035

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P70/50
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

Examples of the present technology may include a method of making a non-woven fiber mat. The wet nonwoven fiber mat may include a first plurality of first glass fibers and a second plurality of second glass fibers. The first plurality of first glass fibers may have nominal diameters of less than 5 μm, and the second plurality of second glass fibers may have nominal diameters of greater than 6 μm. The method may further include curing the binder composition to produce the nonwoven fiber mat. The nonwoven fiber mat may have an average 40 wt. % sulfuric acid wick height of between about 1 cm and about 5 cm after exposure to 40 wt. % sulfuric acid for 10 minutes conducted according to method ISO8787, and the nonwoven fiber mat may have a total normalized tensile strength greater than 2 (lbf/in)/(lb/sq) for a sq (100 ft2).

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.