Patent · US Active

Small pore size nonwoven mat with hydrophilic/acid resistant filler used in lead acid batteries and applications therefor

US9755205B2 · kind B2 · utility

0Cited by
1References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 9, 2015
Grant dateSep 5, 2017
Priority date
Expiry dateOct 1, 2035

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

According to one embodiment, a nonwoven fiber mat includes between 10% and 50% by weight of a plurality of first glass fibers having an average diameter of less than 5 μm and between 50% and 90% by weight of a plurality of second glass fibers having an average diameter of greater than 6 μm. The nonwoven fiber mat also includes an acid resistant binder that binds the first and second glass fibers together. The nonwoven fiber mat has an average pore size of between 1 and 100 μm and exhibits an air permeability of below 100 cubic feet per minute per square foot (cfm/ft2) as measured by the Frazier test at 125 Pa according to ASTM Standard Method D737.