Complex oxide, method for producing same, and exhaust gas purifying catalyst
US9757711B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jul 2, 2015 |
| Grant date | Sep 12, 2017 |
| Priority date | — |
| Expiry date | Jul 2, 2035 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01P2006/16
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
Disclosed are a composite oxide which is capable of maintaining a large volume of pores even used in a high temperature environment, and which has excellent heat resistance and catalytic activity, as well as a method for producing the composite oxide and a catalyst for exhaust gas purification employing the composite oxide. The composite oxide contains cerium and at least one element selected from aluminum, silicon, or rare earth metals other than cerium and including yttrium, at a mass ratio of 85:15 to 99:1 in terms oxides, and has a property of exhibiting a not less than 0.30 cm3/g, preferably not less than 0.40 cm3/g volume of pores with a diameter of not larger than 200 nm, after calcination at 900° C. for 5 hours, and is suitable for a co-catalyst in a catalyst for vehicle exhaust gas purification.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.