Patent · US Active

Method for recovering ruthenium from spent ruthenium-based catalyst carried on aluminum oxide

US9758844B2 · kind B2 · utility

0Cited by
1References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 5, 2014
Grant dateSep 12, 2017
Priority date
Expiry dateNov 26, 2035

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P10/20
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for recovering ruthenium from a spent ruthenium-based catalyst carried on aluminum oxide includes: drying, calcining, and cooling a spent catalyst; grinding the spent catalyst into black powder; placing the black powder in a fluidized bed reactor, purging the reactor with hydrogen and heating the black powder to obtain ruthenium metal, then heating the black powder in a mixed atmosphere of oxygen and ozone to obtain RuO4 gas; absorbing the RuO4 gas with a sufficient amount of hydrochloric acid to obtain a H3RuCl6 solution; adding an excess oxidant to the H3RuCl6 solution to oxidize the H3RuCl6 into H2RuCl6; adding excess NH4Cl to the H2RuCl6 and then filtering, and washing the filter cake to obtain solid (NH4)2RuCl6; and reducing the solid (NH4)2RuCl6 by hydrogen to obtain ruthenium metal.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.