Methods for artificially aging aluminum-zinc-magnesium alloys, and products based on the same

US9765419B2 · kind B2 · utility

0Cited by
8References
33Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 12, 2014
Grant dateSep 19, 2017
Priority date
Expiry dateApr 29, 2035

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/002
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 310° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.