Abstract

The present invention relates to the use of comb polymers comprising, in the main chain, repeat units which are derived from polyolefin-based macromonomers, and repeat units which are derived from low molecular weight monomers selected from the group consisting of styrene monomers having 8 to 17 carbon atoms, alkyl (meth)acrylates having 1 to 10 carbon atoms in the alcohol group, vinyl esters having 1 to 11 carbon atoms in the acyl group, vinyl ethers having 1 to 10 carbon atoms in the alcohol group, (di)alkyl fumarates having 1 to 10 carbon atoms in the alcohol group, (di)alkyl maleates having 1 to 10 carbon atoms in the alcohol group and mixtures of these monomers, where the molar degree of branching is in the range of 0.1 to 10 mol % and the comb polymer comprises a total of at least 80% by weight, based on the weight of the repeat units, of repeat units which are derived from polyolefin-based macromonomers and repeat units which are derived from low molecular weight monomers selected from the group consisting of styrene monomers having 8 to 17 carbon atoms, alkyl (meth)acrylates having 1 to 10 carbon atoms in the alcohol group, vinyl esters having 1 to 11 carbon atoms in the ac…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.