Patent · US Active

Titanium raw material for lithium titanate production and method for producing lithium titanate using same

US9786912B2 · kind B2 · utility

0Cited by
1References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 26, 2012
Grant dateOct 10, 2017
Priority date
Expiry dateJan 9, 2033

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/2982
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

The invention provides a low-cost, efficient method for producing lithium titanate that is useful for applications in electric storage devices. The desired lithium titanate can be obtained by heating at least (1) titanium oxide having a BET single point specific surface area of 50 to 450 m2/g based on nitrogen adsorption and (2) a lithium compound. Preferably the titanium oxide and lithium compound are heated together with (3) a lithium titanate compound having the same crystal structure as the desired lithium titanate. Preferably these ingredients are dry-mixed before heating.