Abstract
A method providing a first tubular workpiece having a first weld surface at an end thereof, and a second tubular workpiece having a second weld surface at an end thereof; aligning the workpieces on a common axis with the weld surfaces facing each other, rotating one workpiece about the axis relative to the other workpiece, and engaging the first and second weld surfaces such that the rotation raises the temperature at the weld surfaces to create a weld interface; and ceasing the rotation and allowing the weld interface to cool to weld the workpieces together at the interface. The first weld surface is an apex region of an annular projection at the end of the first workpiece, on a longitudinal section through the aligned workpieces the annular projection having a profile in which radially inner and outer side surfaces of the annular projection taper towards the apex region.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.