Method for producing titanium-doped synthetic quartz glass
US9796617B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Feb 7, 2014 |
| Grant date | Oct 24, 2017 |
| Priority date | — |
| Expiry date | Feb 7, 2034 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC03C2203/40
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
A method for producing titanium-doped synthetic quartz glass includes: The liquid SiO2 feedstock material comprises at least one additional component made of the polyalkylsiloxane D3 having a weight fraction of mD3 and one additional component made of the polyalkylsiloxane D5 having a weight fraction of mD5 at a weight ratio of mD3/mD5 in a range of 0.01 to 1, and the liquid SiO2 feedstock material provided is evaporated while maintaining the weight ratio of mD3/mD5 and at least 99% by weight thereof are evaporated to form the gaseous SiO2 feedstock vapor.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.