Patent · US Active

Temperable three layer antirefrlective coating, coated article including temperable three layer antirefrlective coating, and/or method of making the same

US9796619B2 · kind B2 · utility

18Cited by
16References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 8, 2010
Grant dateOct 24, 2017
Priority date
Expiry dateJun 22, 2035

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC03C2218/365
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A coated article includes a temperable antireflection (AR) coating that utilizes medium and low index (index of refraction “n”) layers having compressive residual stress in the AR coating. In certain example embodiments, the coating may include the following layers from the glass substrate outwardly: silicon oxynitride (SiOxNy) medium index layer/high index layer/low index layer. In certain example embodiments, depending on the chemical and optical properties of the high index layer and the substrate, the medium and low index layers of the AR coating are selected to cause a net compressive residual stress.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.