A sulfur concrete has constituents that include a coarse aggregate in an amount in a range of 40-50 wt % of the weight of the sulfur concrete, a fine aggregate in an amount in a range of 20-40 wt % of the weight of the sulfur concrete, a fine filler in an amount in a range of 8-12 wt % of the weight of the sulfur concrete, and a binder in an amount in a range of 12-20 wt % of the weight of the sulfur concrete. The binder includes elemental sulfur in an amount in a range of 25-60 wt % of the weight of the binder and asphalt in an amount in a range of 40-75 wt % of the weight of the binder.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.