Patent · US Active

Method for hot-dip coating of a steel flat product

US9803270B2 · kind B2 · utility

0Cited by
9References
13Claims
0Family size

Assignees

Inventors

Key dates

Filing dateDec 13, 2012
Grant dateOct 31, 2017
Priority date
Expiry dateMay 3, 2034

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC23C2/40
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method which allows process-stable hot-dip coating of Ni-alloy steel flat products in a cost- and resource-effective manner, including the following steps: a) provision of a steel flat product obtained by cold- or hot-rolling; b) within 1-30 s, heating the steel flat product to a holding temperature between 700 and 1100° C., under a heating atmosphere of N2; c) holding the steel flat product at the holding temperature for a holding duration of 10-120 s under a holding atmosphere of N2; d) cooling the steel flat product from the holding temperature to a strip inlet temperature of 430-800° C.; and e) passing the steel flat product through an inlet zone, in which an inert or reducing inlet atmosphere predominates, and passing the steel flat product through a melt bath, wherein TP1>TP2>TP4.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.