Patent · US Active

Method of manufacturing a superconductive cable

US9806511B2 · kind B2 · utility

0Cited by
2References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 18, 2014
Grant dateOct 31, 2017
Priority date
Expiry dateJul 29, 2035

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T29/49014
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A method is provided for manufacturing a superconductive cable equipped with means for compensating length changes caused by temperature changes which occur when the cable is cooled from room temperature to work temperature and vice-versa. A superconductive cable (SK) with a tubular, central carrier (1) is used which is surrounded by at least one superconductive conductor. Arranged in the carrier (1) is at least one tension-proof strand (2) arranged over the entire length of the carrier (1). Cable (SK) is initially wound, including strand (2), at room temperature onto a coil (SP). Subsequently, the strand (2) is immovably fastened to the two ends of the cable (SK) and the cable (SK) is subsequently wound off the coil (SP).

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.