Patent · US Active

Case hardening steel with excellent fatigue properties

US9809875B2 · kind B2 · utility

0Cited by
0References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 18, 2013
Grant dateNov 7, 2017
Priority date
Expiry dateAug 29, 2034

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D9/40
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A case hardening steel includes as a chemical composition, by mass %, C: 0.10% to 0.40%, Si: 0.01% to 0.80%, Mn: 0.1% to 1.5%, Cr: 0.35% to 2.0%, Al: 0.01% to 0.05%, REM: 0.0001% to 0.050%, O: 0.0001% to 0.0030%, Ca: 0.0050% or less as necessary, Ti: less than 0.005%, N: 0.015% or less, P: 0.03% or less, S: 0.01% or less, and the balance consists of Fe and impurities. The case hardening steel also includes a composition inclusion which is an inclusion containing REM, O, S, and Al, or an inclusion containing REM, Ca, O, S, and Al, to which TiN is adhered.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.