Patent · US Active

Self-assembly of coatings utilizing surface charge

US9809896B2 · kind B2 · utility

0Cited by
8References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 20, 2015
Grant dateNov 7, 2017
Priority date
Expiry dateJan 20, 2035

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldMeasurement
  • WIPO sectorInstruments

Abstract

An apparatus and method for measuring the isoelectric pH for materials deposited on or otherwise affixed onto and in contact with an electrode surface, and a method for utilizing the isoelectric pH to form nanometer thickness, self-assembled layers on the material, are described. Forming such layers utilizing information obtained about the isoelectric pH values of the substrate and the coating is advantageous since the growth of the coating is self-limiting because once the surface charge has been neutralized there is no longer a driving force for the solid electrolyte coating thickness to increase, and uniform coatings without pinhole defects will be produced because a local driving force for assembly will exist if any bare electrode material is exposed to the solution. The present self-assembly procedure, when combined with electrodeposition, may be used to increase the coating thickness. Self-assembly, with or without additional electrodeposition, allows intimate contact between the anode, electrolyte and cathode which is required for successful application to solid-state batteries, as an example.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.