Recycling positive-electrode material of a lithium-ion battery
US9825341B2 · kind B2 · utility
Assignee
Inventor
Key dates
| Filing date | Aug 6, 2015 |
| Grant date | Nov 21, 2017 |
| Priority date | — |
| Expiry date | Oct 20, 2035 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02W30/84
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
Examples are disclosed of methods to recycle positive-electrode material of a lithium-ion battery. In one example, the positive-electrode material is heated under pressure in a concentrated lithium hydroxide solution. After heating, the positive-electrode material is separated from the concentrated lithium hydroxide solution. After separating, the positive electrode material is rinsed in a basic liquid. After rinsing, the positive-electrode material is dried and sintered.