Method and composition for sequestration of arsenic
US9849438B2 · kind B2 · utility
1Cited by
2References
14Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Mar 31, 2016 |
| Grant date | Dec 26, 2017 |
| Priority date | — |
| Expiry date | Mar 31, 2036 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/20
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
There is provided a method and composition for sequestration of arsenic, the method comprising melting an arsenic-containing material in the presence of iron oxide and glass, and yielding a resulting glass incorporating arsenic. The resulting glass has an arsenic content comprised in a range between 1 and 25% w/w and an iron content comprised in a range between 8 and 20% w/w.