Method for producing a lithium microbattery
US9882183B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Sep 16, 2014 |
| Grant date | Jan 30, 2018 |
| Priority date | — |
| Expiry date | Sep 16, 2034 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P70/50
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
The fabrication method of a lithium microbattery provides for use of a substrate successively covered by: a cathode, a solid electrolyte, and a first electrically conducting layer made from a material configured to combine with the lithium atoms. The first layer is devoid of contact with the cathode. The method further includes formation of a second electrically conducting layer configured to form a diffusion barrier for the lithium atoms. The second layer is electrically connected to the first layer and leaves at least a part of the first layer uncovered, the part being facing the electrolyte. Electrochemical deposition of a lithium anode is then performed from germination from the first and second electrically conducting layers.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.