Patent · US Active

Corrosion inhibitors for Fe2P structure magnetocaloric materials in water

US9887027B2 · kind B2 · utility

1Cited by
3References
21Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 25, 2014
Grant dateFeb 6, 2018
Priority date
Expiry dateNov 10, 2034

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02B30/00
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

Use of a composition (A) having a pH of at least 8 at 25° C. containing at least 50 wt.-% of water or a water containing solvent mixture, at least 0.1 mol/m3 of at least one water soluble silicate, optionally at least one molybdate, optionally at least one phosphonate, optionally at least one azole, optionally at least one additional freezing point depressing salt, optionally at least one phosphate, and optionally at least one nitrate, as heat carrier medium for magnetocaloric materials of formula (I) (AyB1−y)2+uCwDxEz (I) where: A is Mn or Co, B is Fe, Cr or Ni, C is Ge, As or Si, D is different from C and is selected from P, B, Se, Ge, Ga, Si, Sn, N, As and Sb, E may be same or different from C and D and is selected from P, B, Se, Ge, Ga, Si, Sn, N, As and Sb.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.