Method for manufacturing a wide bandgap junction barrier schottky diode

US9887086B2 · kind B2 · utility

1Cited by
2References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 7, 2017
Grant dateFeb 6, 2018
Priority date
Expiry dateJun 7, 2037

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH10D64/64
  • WIPO fieldSemiconductors
  • WIPO sectorElectrical engineering

Abstract

A method for manufacturing a wide bandgap junction barrier Schottky diode having an anode side and a cathode side is provided, wherein an (n+) doped cathode layer is arranged on the cathode side, at least on p doped anode layer is arranged on the anode side, an (n−) doped drift layer is arranged between the cathode layer and the at least one anode layer, which drift layer extends to the anode side, wherein the following manufacturing steps are performed: a) providing an (n+) doped wide bandgap substrate, b) creating the drift layer on the cathode layer, c) creating the at least one anode layer on the drift layer, d) applying a first metal layer on the anode side on top of the drift layer for forming a Schottky contact, characterized in, that e) creating a second metal layer on top of at least one anode layer, wherein after having created the first and the second metal layer, a metal layer on top of the at least one anode layer has a second thickness and a metal layer on top of the drift layer has a first thickness, wherein the second thickness is smaller than the first thickness, f) then performing a first heating step at a first temperature, by which due the second thickness being…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.