Method for manufacturing hot stamped body having vertical wall and hot stamped body having vertical wall
US9896736B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 28, 2016 |
| Grant date | Feb 20, 2018 |
| Priority date | — |
| Expiry date | Oct 28, 2036 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC21D2211/009
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
The present invention provides a method for manufacturing a hot stamped body having a vertical wall, the method including: a hot-rolling step; a coiling step; a cold-rolling step; a continuous annealing step; and a hot stamping step, in which the continuous annealing step includes a heating step of heating the cold-rolled steel sheet to a temperature range of equal to or higher than Ac1° C. and lower than Ac3° C.; a cooling step of cooling the heated cold-rolled steel sheet from the highest heating temperature to 660° C. at a cooling rate of equal to or less than 10° C./s; and a holding step of holding the cooled cold-rolled steel sheet in a temperature range of 550° C. to 660° C. for one minute to 10 minutes.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.