Patent · US Active

Steel wire rod having high strength and ductility and method for producing same

US9896750B2 · kind B2 · utility

0Cited by
1References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 28, 2012
Grant dateFeb 20, 2018
Priority date
Expiry dateDec 26, 2033

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/001
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

There are provided a steel wire rod for ultra-high-strength parts such as automobile engine bolts or structural mechanical parts, and a method for producing the steel wire rod. The steel wire rod having high strength and ductility includes, by wt %, carbon (C): 0.7% to 0.9%, manganese (Mn): 13% to 17%, copper (Cu): 1% to 3%, and the balance of iron (Fe) and inevitable impurities.