Process for manufacturing press-hardened coated steel parts and precoated sheets allowing these parts to be manufactured

US9909194B2 · kind B2 · utility

6Cited by
4References
21Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 6, 2013
Grant dateMar 6, 2018
Priority date
Expiry dateJul 15, 2034

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC23C2/40
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A cold-rolled sheet is provided. The cold-rolled sheet is annealed and pre-coated for the fabrication of press hardened parts, composed of a steel substrate for heat treatment with a carbon content C0 between 0.07% and 0.5%, expressed by weight, and a metal pre-coating on at least the two principal faces of the steel substrate. The substrate comprises a decarburized area on the surface of each of the two principal faces. The depth p50% of the decarburized area is between 6 and 30 micrometers, and p50% is the depth at which the carbon content is equal to 50% of the content C0. The sheet does not contain a layer of iron oxide between the substrate and the metal pre-coating. Processes are also provided.