Method for producing a secondary battery and the metal contaminant deactivation of the same
US9917331B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 2, 2013 |
| Grant date | Mar 13, 2018 |
| Priority date | — |
| Expiry date | Oct 2, 2033 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T29/49108
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
Provided are a secondary battery having a configuration with which localized metal contaminant precipitation at the negative electrode can be reliably inhibited in less time, and a method for producing a secondary battery that allows reliable deactivation of metal contaminant in less time. The battery comprises a positive electrode, a negative electrode, and a separator placed between the two electrodes. The separator has an air resistance Rp≦100 sec in an in-plane direction vertical to its thickness direction and an air resistance Rt>Rp in the thickness direction. The method comprises a minimal charging step where the cell is charged to 0.01% to 0.5% capacity over at least one hour to obtain a state of charge where the positive and negative electrode potentials are at or above the oxidation and reduction potentials of a probable metal contaminant, respectively; and a step of performing initial conditioning charging.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.