Sintered molybdenum carbide-based spray powder
US9919358B2 · kind B2 · utility
Assignee
Inventor
Key dates
| Filing date | Oct 1, 2014 |
| Grant date | Mar 20, 2018 |
| Priority date | — |
| Expiry date | Oct 1, 2034 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC23C4/134
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A sintered spray powder includes from 5 to 50 wt.-% of a metallic matrix, from 50 to 95 wt.-% of a hard material, and from 0 to 10 wt.-% of a wear-modifying oxide, each based on the total weight of the sintered spray powder. The metallic matrix comprises from 0 to 20 wt.-% of molybdenum based on the total weight of the metallic matrix. The hard material comprises at least 70 wt.-% of molybdenum carbide based on the total weight of the hard material. An average particle diameter of the molybdenum carbide in the sintered spray powder is <10 μm, determined in accordance with ASTM E112.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.