Method for producing purified alkali silicate aqueous solution and silica sol
US9938155B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 20, 2015 |
| Grant date | Apr 10, 2018 |
| Priority date | — |
| Expiry date | May 2, 2035 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01P2004/64
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
To provide a method for producing an alkali silicate aqueous solution containing a reduced amount of foreign substance of plate-like fine particles and a method for producing a silica sol containing a reduced amount of foreign substance of plate-like fine particles. A method for producing an alkali silicate aqueous solution fulfilling the following condition: the existing amount of plate-like fine particles having a length of one side of 0.2 to 4.0 μm and a thickness of 1 to 100 nm is determined to be 0 to 30%. The method for producing an alkali silicate aqueous solution includes the steps of adjusting a silica concentration of an alkali silicate aqueous solution to 0.5 to 10.0% by mass and filtering the alkali silicate aqueous solution through a filter having a removal rate of particles with a primary particle size of 1.0 μm of 50% or more.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.