Manufacturing method of sintered alloy, compact for sintering, and sintered alloy

US9950369B2 · kind B2 · utility

1Cited by
0References
10Claims
0Family size

Assignees

Inventors

Key dates

Filing dateFeb 1, 2017
Grant dateApr 24, 2018
Priority date
Expiry dateFeb 1, 2037

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/12979
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Mixed powder that contains first hard particles, second hard particles, graphite particles, and iron particles is used to manufacture a sintered alloy. The first hard particle is a Fe—Mo—Cr—Mn based alloy particle, the second hard particle is a Fe—Mo—Si based alloy particle. The mixed powder contains 5 to 50 mass % of the first hard particles, 1 to 8 mass % of the second hard particles, and 0.5 to 1.0 mass % of the graphite particles when total mass of the first hard particles, the second hard particles, the graphite particles, and the iron particles is set as 100 mass %.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.