Recovering a caustic solution via calcium carbonate crystal aggregates

US9975100B2 · kind B2 · utility

4Cited by
6References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 9, 2014
Grant dateMay 22, 2018
Priority date
Expiry dateOct 8, 2036

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P70/10
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

Techniques for converting a portion of a carbonate to hydroxide include receiving an alkaline carbonate solution that includes between 0.1M (moles per liter of solution) to 4.0M hydroxide and between 0.1M to 4.1M carbonate; reacting, in a slaking process, quicklime (CaO) and a low carbonate content fluid to yield a slurry of primarily slaked lime (Ca(OH)2); and reacting the Ca(OH)2 slurry and the alkaline carbonate solution to grow calcium carbonate (CaCO3) crystal aggregates of 0.0005 mm3 to 5 mm3 in volume in a fluidized-bed reactive crystallizer.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.