Patent · US Active

Methods for making a solid electrolyte interface layer on a surface of an electrode

US9979008B2 · kind B2 · utility

32Cited by
6References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 4, 2015
Grant dateMay 22, 2018
Priority date
Expiry dateMay 30, 2036

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P70/50
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

In an example of the method for making a solid electrolyte interface (SEI) layer on a surface of an electrode, the electrode is exposed to an electrolyte solution in an electrochemical cell. The electrolyte solution includes either i) an organo-polysulfide additive having a formula RSnR′ (n≥2), wherein R and R′ are independently selected from a methyl group, an unsaturated chain, a 3-(Trimethoxysilyl)-1-propyl group, or a 4-nitrophenyl group, or ii) a fluorinated organo-polysulfide additive having a formula RSnR′ (n≥2), wherein R and R′ can be the same or different, and wherein R and R′ each have a general formula of CxHyF(2x−y+1), where x is at least 1 and y ranges from 0 to 2x. A voltage or a load is applied to the electrochemical cell.