Abrasion resistant steel plate having excellent low-temperature toughness and excellent corrosive wear resistance

US9982331B2 · kind B2 · utility

1Cited by
2References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 13, 2013
Grant dateMay 29, 2018
Priority date
Expiry dateSep 17, 2034

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/008
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

An abrasion resistant steel plate which possesses excellent abrasion resistance, excellent low-temperature toughness and excellent corrosive wear resistance. The abrasion resistant steel plate has the composition comprising by mass %: 0.10% to 0.20% C, 0.05% to 1.00% Si, 0.1% to 2.0% Mn, 0.020% or less P, 0.005% or less S, 0.005% to 0.100% Al, one or two kinds of components selected from a group consisting of 0.05% to 2.0% Cr and 0.05% to 1.0% Mo, and remaining Fe and unavoidable impurities as a balance. Content of solute Cr in steel (Crsol) and the content of solute Mo in steel (Mosol) satisfy the formula 0.05≥(Crsol+2.5Mosol)≥2.0. Steel plate has a structure where an as-quenched martensitic phase forms a main phase and a grain size of prior austenite grains is 30 μm or less, and surface hardness of the steel plate is 360 or more at Brinel hardness HBW10/3000.